Skip Navigation

C-steel

Alloy steel for quenching and tempering and spring steel

DIN EN 10 083, DIN EN 10 084

Steel grade designation Standard designation THICKNESS1
from _ to in mm
WIDTH1
from _ to in mm
16MnCr5 16MnCr5 2.00 – 10.00 50 – 1,600
20MnCr5 20MnCr5 2.00 – 10.00 50 – 1,600
34CrMo4 34CrMo4 2.00 – 8.00 100 – 1,600
42CrMo4 42CrMo4 2.00 – 8.00 100 – 1,600
51CrV4 51CrV4 2.00 – 8.00 100 – 1,600
58CrV4 Special mill grade 2.00 – 8.00 100 – 1,600
80CrV2* Special mill grade 2.00 – 8.00 100 – 1,600
75Cr1 Special mill grade 2.00 – 8.00 100 – 1,600
74NiCr2 Special mill grade 2.00 – 8.00 100 – 1,600

* Analytical based on DIN EN 10 132-4

1 Not all thickness and width combinations possible